Products and Services
Introduction
Materials
Piezo Cylinders
Air Transducers
Piezo Buzzers
Nebulizers (Fluid Atomizers)
Ultrasonic Cleaning Transducers
Disc Benders
Piezo Ignitors
Stripe Actuators
Stack Actuators
Single Crystals
Alumina Parts/Saggers
d33 Testers
Theory/Applications Book
Services
Product Design

Search Our Site

Home | News | Contact | Site Map | Piezo Theory | Materials | Products/Services | Order 


Alumina / Zirconia Ceramics
High Temperature Saggers

Now Available!!  Alumina Balls and a Alumina Powders
Data Sheet Coming Soon, Contact APC for details

  • excellent mechanical and electrical properties:
    • high temperature capability
    • high density / high hardness
    • excellent corrosion / abrasion resistance
    • excellent electrical properties
    • good thermal cycling ability
  • suitable for vacuum applications
  • Al2O3 materials non-toxic and inert
  • forming capabilities for making intricate parts
  • high volume production capacity
  • competitive pricing
  • fast delivery

Typical Applications

  • valves and pumps
  • bearings
  • nozzles
  • pistons
  • wire drawing dies
  • refractory parts
  • abrasion resistant elements
  • mechanical seals
  • thread guides
  • tool bits
  • crucibles
  • saggers
  • OEM specifications

Standard High Temperature Alumina Saggers and Lids (99.4% alumina)

Custom Sized / Custom Shaped Saggers
We can design and custom produce saggers for specific requirements, from alumina powders of 90 to 99+% purity. Please contact an APCI representative to discuss your needs.

Characteristics of Alumina and Zirconia Ceramic Products from APCI.
These materials have excellent mechanical, chemical, thermal, and electronic properties, for outstanding performance in diverse, demanding applications.

Specifications: Powder-Quelled Fine Structure Ceramics
  Al2O3 Toughness
Strengthened
Al2O3
ZrO2
Content (%) to 99 Al/Zr = 87/13 Zr/Y = 97/3
Density (g/cm3) 3.9 - 4.0 4.0 - 4.1 5.9 - 6.0
Hardness (HRA) 80 - 90 90 - 92 90 - 91
Bend Strength (MPa) 3300 3350 3800
Wear Capacity average good excellent

Specifications: Molding Products (Crucibles)
  pure Al2O3
Content (%) >99.4
Density (g/cm3) 3.8 - 3.9
Hardness (HRA) 87 - 89
Bend Strength (MPa) 250 - 300
Fireproof Extent (°C) 1650

 
Home | News | Contact | Site Map | Piezo Theory | Materials | Products/Services | Order