Ultrasonic Cleaning Transducers

(Catalog No. 90-)
  • high efficiency
  • large amplitude
  • low heat
  • stable output unaffected by variations in load
  • competitive pricing
  • fast delivery

Typical Applications

  • ultrasonic cleaning apparatus



Request A Quote

High mechanical quality ensures that these sandwich-type ultrasonic transducers offer high electro-acoustical efficiency and low heat generation. The mechanical connection of the piezoelectric elements assures a large amplitude output. Choose 28 kHz, 40 kHz, 80 kHz, or 120 kHz resonance frequency.

Standard Ultrasonic Cleaning Transducers
Mechanical
Quality
(Qm)
Coupling
(Kp)
(%)
Capacitance
(1 kHz)
(nf)
Impedance
(ohm)
Motion
Admittance
(m)
Allowable
Vibration
(cm/sec)
Power
(watts)
28 kHz -- APCI Catalog No. 90-4040  .pdf Spec. Sheet
800   ≥ 55 3.8 ≤ 50 60 ≤ 25 50
40 kHz -- APCI Catalog No. 90-4050  .pdf Spec. Sheet
800   ≥ 55 3.8 ≤ 50 65 ≤ 50 50
80 kHz -- APCI Catalog No. 90-4060  .pdf Spec. Sheet
≥ 1000   ≥ 55 3.7 ≤ 50     80
120 kHz -- APCI Catalog No. 90-4070  .pdf Spec. Sheet
≥ 1000   ≥ 55 3.7 ≤ 50     80
Other sizes available upon request - please inquire
To download all of the Standard Ultrasonic Cleaning Transducer spec sheets at one time click here (124k .pdf)

Ultrasonic Transducer Generator Specification Download

To download the APCI Ultrasonic Transducer Generator spec sheet click here (35k .pdf)


 