| Characteristic | Type II |
| Relative Dielectric Constant/K | 1800 |
| Dielectric DissipationFactor / tanδ (%) | 2.0 |
| Curie Point / TC(°C) | 300 |
| Electromechanical CouplingFactor / k31 (%) | >0.35 |
| PiezoelectricCharge Constant (pC/N) | |
| d33 | 330 |
| -d31 | 175 |
| Density / ρ (g/cm3) | 7.5 |
| Mechanical Quality Factor / Qm | 85 |