Archive for October, 2015
Ceramic Manufacturing Series – Pressing PZT Powders
Pressing PZT Powders
Starting with high quality PZT powders makes pressing a little easier. Brian Julius, V.P. Manufacturing / Materials Engineer Ron Staut, V.P. Technology All ceramic parts begin as a powder in one form or another. How that powder is transformed into a starting shape, however, can differ. It is the compaction throughRead More...