Products and Services
Introduction
Materials
Piezo Cylinders
Air Transducers
Piezo Buzzers
Nebulizers (Fluid Atomizers)
Ultrasonic Cleaning Transducers
Disc Benders
Piezo Ignitors
Stripe Actuators
Stack Actuators
Single Crystals
Alumina Parts/Saggers
d33 Testers
Theory/Applications Book
Services
Product Design

Search Our Site

Home | News | Contact | Site Map | Piezo Theory | Materials | Products/Services | Order 


Stripe™ Actuators

(Catalog No. 40-)

Bilaminar, flexing actuators featuring:

  • large deflections
  • useful blocking forces
  • surfaces protected from environmental hazards
  • electrical leads / no leads
  • custom dimensions available
  • competitive pricing
  • fast delivery

Typical Applications
Use Stripe actuators in applications that demand sensitivity
or a large response:

  • needle control in textile weaving
  • Braille machines
  • accelerometers
  • opening / closing valves
  • small-volume pumping devices
  • switching applications - touch switches -
    making / breaking electrical contact
  • cooling devices for electronics (no electromagnetic noise)



Request A Quote

Background information about Stripe actuators

Custom Design and Engineering Services
If the dimensions or performance characteristics of standard Stripe actuators do not fit your needs, we can custom-manufacture these actuators to your specifications. Before you request custom products, however, we recommend you evaluate standard Stripe actuators for your application by varying the free length, the method of mounting, and/or the applied voltage. The relationships in technical note Performance of Stripe Actuators will help you in your evaluation. If you find that standard Stripe actuators will not provide the performance you need, simply contact an APCI representative to discuss alternatives.

Stripe Actuators
Dimensions
(mm)
Free
Length
(mm)
Total
Deflection
(mm)
Blocking
Force
(N)
Resonance
Frequency
(Hz)
Capacitance
(pF)
Long Wide Thick
 Catalog No. 40-1010 (600/200/0.60-SA)
 60.0 20.0 0.60 53 >2.5 >0.25 65 170,000
Catalog No. 40-1035 (490/018/0.60-SA)
49.0 1.8 0.60 42 >1.5 >0.03 110 25,000
Catalog No. 40-1025 (490/021/0.60-SA)
49.0 2.1 0.60 42 >1.5 >0.05 110 15,000
Catalog No. 40-1040 (400/200/0.60-SA)
40.0 20.0 0.60 33 >1.0 >0.40 175 115,000
Catalog No. 40-1055 (350/025/0.60-SA)
35.0 2.5 0.60 28 >0.7 >0.06 245 12,000
Deflections and blocking forces measured at driving voltage of 150 V (maximum) in direction of polarization.
Operating temperature: -25°C to 70°C; storage temperature: -40°C to 85°C.

 
Home | News | Contact | Site Map | Piezo Theory | Materials | Products/Services | Order
 ©1998-2009 APC International, Ltd.  All rights reserved.