Piezoelectric Air Transducers

Custom Design and Engineering Services of Piezoelectric Ultrasonic Air Transducers

We can custom design air transducers for unique requirements and electrical properties. If the design you need is not listed here, please contact an APCI representative to discuss your specifications.

Our air transducer applications consist of a piezoelectric ceramic element, mounted in an aluminum, plastic, or environmental (sealed) housing. These piezoelectric transducers offer high sensitivity, superb sound pressure level (SPL), and stable electrical and mechanical characteristics, at a choice of bandwidths and vary in frequencies and amplitudes. Environmental transducers may act as both transmitter and receiver; or separate transmitter or receiver.

Request Air Transducer Quote

Ultrasonic Air Transducer Module

APC offers an ultrasonic air transducer module (Cat# 10-3300) for use in conjunction with our standard 300 kHz air transducer (Cat# 10-3310). APC’s air transducer module can be used for short distance measurement, close object detection, and level sensing. View the product spec sheet for more details.

APCI
Catalog
No.
Center /
Resonance
Frequency
(kHz)
Transmitter
/ Receiver
Output SPL
(at 10V)
(dB)
Sensitivity
(dB)
Bandwidth
(-6 dB)
(kHz)
Outer
Diameter
(mm)
Housing  
10-3210
40 kHz Sonar Ranging Module (50-1500 cm)
Spec Sheet
10-3240
40 kHz Sonar Ranging Module (25-150 cm)
Spec Sheet
10-3300
300 kHz Air Transducer Module with Driver Board & Transducer
Spec Sheet
10-1011 25 ±1 T >112 — 4 16 Aluminum Spec Sheet
10-1016 25 ±1 R — ≥-65 3.5 16 Aluminum Spec Sheet
10-1036 40 ±1 T >112 — 4 10 Aluminum Spec Sheet
10-1041 40 ±1 R — ≥-69 2 10 Aluminum Spec Sheet
10-1061 40 ±1 T >115 — 4 12.7 Aluminum Spec Sheet
10-1066 40 ±1 R — ≥-67 2 12.7 Aluminum Spec Sheet
10-1096 40 ±1 T >119 — 4 16 Aluminum Spec Sheet
10-1101 40 ±1 R — ≥-65 3.5 16 Aluminum Spec Sheet
10-1106 40 ±1 T >119 — 4 16.1 Plastic Spec Sheet
10-3066 40 ±1 R — ≥-70 3 9.7 Plastic Spec Sheet
10-3111 40 ±1 T >112 — 2.5 9.7 Plastic Spec Sheet
10-3041 40 ±1 T/R >103 >78 1 14 Plastic Spec Sheet
10-3005 40 ±1 T/R >110 ≥-68 2 9.7 Aluminum Spec Sheet
10-3133 40 ±1 T/R >102 ≥78 3 8 Stainless Spec Sheet
10-3155 40 ±1 T/R >115 ≥-68 2 12.7 Aluminum Spec Sheet
10-3165 40 ±1 T/R >117 ≥-65 2 16.2 Aluminum Spec Sheet
10-3170 40 ±1 T/R >117 ≥-65 2 16.2 Plastic Spec Sheet
10-3136 40 ±1 T/R >108 ≥-75 2 18.1 Environmental Spec Sheet
10-3235 40 ±1 T/R >113 ≥-72 2 25.1 Environmental Spec Sheet
10-3310 300 See Spec Sheet 9.8 Plastic Spec Sheet
Custom
Values to be Determined by Customer and APC International
 
a white background with a few lines on it

Contact APC International Today to Discuss Your Piezoelectric Ceramic or Piezo Device Requirements

Discuss Your Transducer Project