Basic Overview of Piezoelectric Materials in Energy Harvesting
Energy harvesting is approaching an interesting technological juncture wherein the power requirements for electronic devices have been reduced while at the same time the efficiency of energy harvesting devices has increased. Out of various
possible energy harvesting technologies, piezoelectric vibration energy harvesting has emerged as a method of
Read More...